WPS and WPQR, and what a buyer should ask for

What a welding procedure specification and its qualification record are, how material groups and process numbers are read, and which documents a buyer should expect before a fabricated part is welded.

Published
24 November 2026
Solution
Contract Steel Fabrication

A drawing says what the weld is. A welding procedure says how it is made so that it is the weld the drawing meant: the process, the consumable, the preparation, the parameters, the preheat and the sequence. This note explains the two documents behind every qualified weld, how their coverage is written down, and what to ask for when you place fabrication work.

The two documents

A welding procedure specification (WPS) is the instruction the welder works to. It fixes the base material, the thickness range, the joint and position, the process, the filler, the shielding gas, the current and voltage ranges, the travel speed, the preheat and the interpass temperature.

A welding procedure qualification record (WPQR) is the proof that the specification produces a sound weld. A test piece is welded to the specification, then examined and tested, by non-destructive testing and by destructive tests such as tensile, bend, impact and macro examination, under EN ISO 15614-1 for steels and EN ISO 15614-2 for aluminium. The record of that test, with its results, is the WPQR. A WPS is only as good as the WPQR that stands behind it.

The two are issued together and controlled as documents: a revision is recorded, and a WPS is withdrawn when its record no longer covers the job. EN 1090-2 at execution class 2 and above, and EN ISO 3834-2, both require welding to be done under qualified procedures of this kind.

How coverage is written

A procedure covers a range, not a single part, and the range is described in three codes that appear on every WPS.

Material groups, ISO/TR 15608. Steels and alloys are grouped by their metallurgy so that one qualification covers the grades that weld alike. Group 1 is structural steel with a specified minimum yield strength up to 460 N/mm², with 1.1 and 1.2 covering S235 to S355 and 1.3 the normalised fine-grain grades; group 2 is thermomechanically rolled fine-grain steel; group 3 is quenched and tempered steel such as S690; group 8 is austenitic stainless steel; group 10 is duplex and super duplex; groups 22 and 23 are the work-hardening and the heat-treatable aluminium alloys.

Process numbers, EN ISO 4063. Each welding process has a number: 135 is MAG welding with a solid wire, 136 with a flux-cored wire, 141 is TIG welding, 111 is manual metal arc. The number on the WPS tells you the process without reading the parameters.

Thickness and position. A WPQR qualifies a thickness range around the test piece, not only the thickness tested, and the positions it was welded in. A procedure qualified on a 20 mm plate in all positions covers a band of thicknesses either side of it.

Already qualified, and qualified for the job

Any grade on your drawing is welded under a qualified procedure. The work we place is made in a production environment that holds over 120 qualified welding procedures (WPS and WPQR), covering the materials most often specified. Grades and thicknesses outside them are qualified for the job, under the same system. Already qualified today:

Material ISO/TR 15608 group Typical grades Process
Structural steels 1.1, 1.2 S235, S275, S355 (EN 10025-2) 135
Fine-grain steels 1.3, 2.1 S460N/NL, S460M/ML (EN 10025-3, -4) 135
Quenched and tempered 3.1 S690Q, S690QL (EN 10025-6) 135
Austenitic stainless 8.1 1.4301 (304), 1.4404 (316L) 141
Duplex and super duplex 10.1, 10.2 1.4462 (2205), 1.4410 (2507) 141, 135
Aluminium alloys 22, 23 EN AW-5083, EN AW-6082 141
Other materials and grades To the specification Qualified for the project, as part of the job 135, 141

The procedures cover plate and tube from 2 to 50 mm in all positions. Welders are qualified to EN ISO 9606-1 for steel and EN ISO 9606-2 for aluminium, International Welding Engineers act as the responsible welding coordinators under EN ISO 14731, and welds are accepted to EN ISO 5817. The grades shown are typical, not the limit of the work; a material or thickness outside this range is qualified as part of the project that needs it.

What to ask for

Before the first weld on your part, the documents to expect are:

  • The WPS for each weld on the drawing, matched to your material specification and thickness, with the WPQR that qualifies it. These are issued for your review before fabrication starts.
  • The welder qualifications for the welders who will make those welds, to EN ISO 9606-1 or 9606-2.
  • The name of the responsible welding coordinator.
  • The inspection plan: which welds are inspected visually, which by penetrant, magnetic particle, ultrasonic or radiographic testing, and the acceptance level to EN ISO 5817.
  • The material certificates to EN 10204 3.1 for the plate and profiles used, and confirmation that the WPS and the welder are recorded against each component.

Send the drawing and the material specification with your enquiry, and the applicable procedures come back with the quotation.

Contract Steel Fabrication: the solution pageAll engineering notes

Next step

Ask the question your component raises.

Send the drawing, the figures or the route, and we will answer from what we have built.

Start a conversation